Sign In | Join Free | My himfr.com
Home > Inconel Alloy >

High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

    Buy cheap High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from wholesalers
     
    Buy cheap High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from wholesalers
    • Buy cheap High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from wholesalers
    • Buy cheap High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from wholesalers
    • Buy cheap High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate from wholesalers

    High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

    Ask Lasest Price
    Brand Name : Victory
    Model Number : Inconel 718
    Certification : ISO9001 ROHS
    Price : Negotiable
    Payment Terms : L/C, T/T, Western Union, MoneyGram
    Supply Ability : 300 tons per month
    Delivery Time : 20~40 Days
    • Product Details
    • Company Profile

    High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

    Inconel 718 Alloy


    Inconel 718 is a precipitation hardened nickel-based alloy designed to display exceptionally high yield, tensile and creep-rupture properties at temperatures up to 1300°F (704°C). The age-hardening response of Inconel 718 permits annealing and welding without spontaneous hardening during heating and cooling. Nickel Alloy 718 has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium.

    Advantages of Inconel 718 Strips


    • High yield strength
    • Excellent high temperature tensile & creep rupture properties
    • Excellent weldability
    • Does not spontaneously harden
    • Outstanding corrosion resistance

    Applications of Inconel 718 Strips


    • Jet engine components
    • Gas turbines
    • Aerospace
    • Plastic injection molded tools
    • High speed airframe parts
    • High temperature bolts & fasteners

    Parameter:

    Chemical Properties of Inconel 718

    Nickel (plus Cobalt) .......................................................50.00-55.00

    Chromium......................................................................17.00-21.00

    Iron .....................................................................................Balance

    Niobium (plus Tantalum)....................................................4.75-5.50

    Molybdenum .....................................................................2.80-3.30

    Titanium.............................................................................0.65-1.15

    Aluminum ..........................................................................0.20-0.80

    Cobalt ...............................................................................1.00 max.

    Carbon..............................................................................0.08 max.

    Manganese .......................................................................0.35 max.

    Silicon ...............................................................................0.35 max.

    Phosphorus.....................................................................0.015 max.

    Sulfur...............................................................................0.015 max.

    Boron ..............................................................................0.006 max.

    Copper..............................................................................0.30 max

    Density 8.19g/cm³ 0.296 lb/in³
    Melting point 1260-1336 2437°F

    SPECIFICATIONS
    Form
    ASTM
    Rod,bar and wire
    B 166
    Plate,sheet and strip
    B 168, B 906
    Seamless pipe and tube
    B 167, B 829
    Welded pipe
    B 517, B775
    Fitting
    B 366
    Billet and bar for reforging
    B 472
    Forging
    B 564

    Inconel series

    Steel grade
    Inconel 600
    Inconel 601
    Inconel 625
    Inconel 718
    Inconel 725
    Inconel X-750
    Corresponding brand
    N06600/2.4816/1Cr15Ni75Fe8/NS312/CY40
    N06601/2.4851/1Cr23Ni60Fe13AI/NS313
    N06625/2.4856/0Cr20Ni65Mo10bN4/NS336
    N07718/2.4668/GH4169
    N07725
    N07750/2.4669/GH4145
    Chemical composition%
    C≤
    0.150
    0.100
    0.100
    0.080
    0.030
    0.080
    Mn≤
    1.00
    1.00
    0.50
    0.35
    0.35
    1.00
    P≤
    /
    /
    0.015
    0.015
    0.015
    /
    S≤
    0.015
    0.015
    0.015
    0.015
    0.010
    0.010
    Si≤
    0.50
    0.50
    0.50
    0.35
    0.20
    0.50
    Cr≤
    14.0-17.0
    21.0-25.0
    20.0-23.0
    17.0-21.0
    19.0-22.5
    14.0-17.0
    Ni≤
    ≥72.0
    58.0-63.0
    ≥58.0
    55.0-59.0
    55.0-59.0
    ≥70
    Mo
    /
    /
    8.0-10.0
    2.8-3.3
    7.0-9.5
    /
    Cu
    ≤0.50
    ≤1.50
    /
    ≤0.30
    /
    ≤0.50
    N
    /
    /
    /
    /
    /
    Nb
    /
    /
    3.15-4.15
    4.75-5.50
    2.75-4.00
    0.70-1.20
    other
    Fe:6.0-10.0
    Al:1.0-1.7
    Co:≤1.0Ai:≤0.40Tr:0.40Fe:≤5.0
    AI:0.20-0.80Ti:0.65-1.15B≤0.006
    Tr:1.0-1.7AI≤0.35
    Co:≤1.0 AI:0.4-1.0Tr:0.25-2.75Fe:5.0-9.0

    Customize size as below

    Shape
    Size(mm)
    WIre
    0.5-7.5
    Rod/Bar
    8.0-200
    Strip
    (0.5-2.5)*(5-180)
    Tube
    custom made
    Plate
    custom made

    contact us

    email:victory@dlx-alloy.com

    Oem service:
    Welcome customized size
    We are experience factory for OEM&ODM service

    High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plateHigh-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plateHigh-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate

    Quality High-strength nickel base superalloy Nickel-chromium alloy 718 strip tape sheet foil plate for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Changzhou Victory Technology Co., Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)